by Admin Admin No Comments

Premium Film Faced Plywood: When 8–12 Reuses Is the Right Target

Premium film faced plywood is the middle grade in the Greenwood formwork range, made for projects that need roughly 8–12 pours from each panel. It pairs a high-quality phenolic film of 135–145 g/m² on both faces with MUF glue containing 15–18% melamine, and the Technical Data Sheet (08/2026) rates it at 12–15 hours in the boiling test.

That puts Premium between Standard (4–8 reuses) and Promax (15–20 reuses). This article sets out the data-sheet values, what the higher melamine content changes compared with Standard, which projects suit Premium, and where Promax becomes the better choice.

Key specifications at a glance (TDS 08/2026)

  • Film: high-quality phenolic film 135–145 g/m², both faces
  • Glue: MUF, melamine 15–18%
  • Boiling test: 12–15 h
  • Expected reuse: 8–12 times (reference value)
  • Thickness: 9–30 mm, tolerance ±0.5 mm
  • Moisture content: ≤12%

Specification (TDS)

The table lists the Premium values from the Greenwood Technical Data Sheet (08/2026). Panel construction and sizes are shared across the four film faced grades.

Property Premium grade
Face / back film High-quality phenolic film 135–145 g/m², both faces
Glue MUF, melamine 15–18%
Boiling test 12–15 h
Expected reuse 8–12 times
Core Eucalyptus, Acacia or mixed hardwood (legally sourced plantation wood)
Plies 5–13, by thickness
Sheet size 1220 × 2440 mm, 1250 × 2500 mm or as requested
Thickness / tolerance 9–30 mm / ±0.5 mm
Moisture content ≤12% (test result: 9.2%)
Edges Sealed with water-resistant paint
Bending strength, along / across grain 60.8 / 35.7 MPa (requirement 50 / 30 MPa)
MOE, along / across grain 6839 / 5474 MPa (requirement 6000 / 4500 MPa)
Bonding strength 0.79 MPa (requirement 0.7 MPa)
Packing Pallet base or wood blocks, PE wrap, steel strapping; custom label on request

Bending strength and MOE are tested to TCVN 12446:2018, bonding to TCVN 12447:2018 and moisture to TCVN 11905:2017. Every Premium result sits above the requirement level in the same row. Treat the reuse range as a reference value: release agent, cleaning, handling and storage on site all move a panel toward the top or bottom of it.

What the extra melamine changes

Short answer: more melamine in the MUF glue line goes with longer boil resistance, stronger bonding and a higher reuse range. Melamine improves how well the glue line holds up to water and heat, which is what concrete pours, curing and cleaning put it through.

Across the Greenwood range, the step from Standard to Premium shows up in every glue-related value on the data sheet:

Value (TDS 08/2026) Standard Premium Promax
Melamine in MUF glue 12% 15–18% 25%
Boiling test 8–12 h 12–15 h 48 h
Bonding strength 0.74 MPa 0.79 MPa 0.84 MPa
Expected reuse 4–8 times 8–12 times 15–20 times
Film Phenolic 165 g/m² High-quality phenolic 135–145 g/m² High-quality phenolic 135–145 g/m²

In practice, the extra glue resistance matters most at the edges and around fixing holes, where water reaches the core first. Sealing every cut edge before use protects that advantage; an unsealed edge can undo it within a few pours.

Projects that suit Premium

Premium fits projects where the panel count is planned around a moderate number of pours and a cleaner finish than Standard is expected. Typical situations:

  • Low- and mid-rise residential or commercial buildings with repeated slab and wall cycles
  • Contractors who move a panel set across two or three smaller projects before replacing it
  • Sites where Standard panels were reaching their limit before the formwork program finished
  • Distributors who need one mid-range grade to cover most formwork enquiries

The planning question is simple: divide the number of pours in the program by the panel set you intend to buy. If each panel needs to survive about 8–12 pours, Premium is the grade to quote first. Below 8 pours, Standard may be enough; above 12, look at Promax.

Premium or Promax: the decision point

Short answer: choose Promax when each panel must go beyond about 12 pours, or when panels stay wet for long periods between pours. Choose Premium when 8–12 pours covers the program.

Premium

MUF with 15–18% melamine, 12–15 h boiling test, 8–12 reuses. Suits moderate programs and mixed project use, with a lower specification to buy into.

Promax

MUF with 25% melamine, 48 h boiling test, 15–20 reuses. Suits high-rise and repetitive pours where panels are cycled many times on one site.

Both grades use the same high-quality phenolic film of 135–145 g/m², so the difference is in the glue line, not the face. If you are unsure which side of 12 pours your program falls, send the pour schedule with your enquiry and we will recommend a grade against it. For the full grade ladder, see Film Faced Plywood Grades and Promax Film Faced Plywood.

FAQ

Why is Premium film lighter than Standard film?

Because they are two different films. Premium uses a high-quality phenolic film of 135–145 g/m² made from better paper, while Standard uses a 165 g/m² film. Film weight on its own says nothing about performance. Glue content, boiling-test hours and bonding strength are what separate the grades.

How many pours can Premium film faced plywood take?

The Greenwood data sheet gives 8–12 reuses for Premium as a reference value. Where a panel lands in that range depends on release agent, cleaning after each pour, careful stripping, edge sealing and dry storage. Rough handling or unsealed cut edges can bring the figure below the range.

What does the 12–15 hour boiling test show?

The boiling test checks how long the glue line holds while samples are boiled in water. Premium panels hold for 12–15 hours, compared with 8–12 hours for Standard and 48 hours for Promax. Longer boil resistance indicates a glue line that stands up better to wet site conditions.

Request the Premium data sheet

Send your thickness, sheet size and pour schedule. Our team will send the Greenwood Premium Technical Data Sheet and a grade recommendation for your program.

Request Premium data sheet →

✉ qc@fomexgroup.vn

☎ +84 877 034 666 (WhatsApp)

FOMEX Global Premium Form film faced plywood →

Greenwood film faced plywood is a product line of FOMEX Global, part of FOMEX Group.

by Admin Admin No Comments

Standard Film Faced Plywood: Specification, Reuse and Where It Fits

Standard is the entry grade in the Greenwood film faced plywood range. It is built for formwork jobs that need a clean concrete finish for a limited number of pours: a 165 g/m² phenolic film on both faces, MUF glue with 12% melamine, an 8–12 hour boiling test and 4–8 reuses.

Knowing where the grade stops is as useful as knowing what it does. The most common complaint about entry-grade panels comes from using them on jobs that needed a higher grade.

Key specifications at a glance (TDS 08/2026)

  • Film: phenolic film 165 g/m², both sides
  • Glue: MUF, 12% melamine
  • Boiling test: 8–12 h
  • Expected reuse: 4–8 times (reference value)
  • Thickness: 9–30 mm, tolerance ±0.5 mm
  • Moisture content: ≤12%

Specification

Source: FOMEX Technical Data Sheet, 08/2026.

Specification Standard film faced plywood
Film Phenolic film 165 g/m², both sides
Glue MUF, 12% melamine
Boiling test 8–12 h
Expected reuse 4–8 times
Core Eucalyptus, acacia or mixed hardwood (legally sourced plantation wood)
Plies 5–13 depending on thickness
Thickness 9–30 mm, tolerance ±0.5 mm
Sheet sizes 1220 × 2440 mm, 1250 × 2500 mm or as requested
Moisture content ≤12%
Edge sealing Water-resistant paint
Packing Pallet base or wooden blocks, PE wrap, steel strapping; custom labels on request

Mechanical values

Property Test result Requirement Test method
Bending strength, length / width 55.2 / 32.6 MPa 50 / 30 MPa TCVN 12446:2018
Modulus of elasticity, length / width 6465 / 4886 MPa 6000 / 4500 MPa TCVN 12446:2018
Bonding strength 0.74 MPa 0.7 MPa TCVN 12447:2018
Moisture content 9.4% — TCVN 11905:2017

Each result sits above the requirement in its row. Treat the figures as reference values from testing: on site, performance also depends on support spacing, load, exposure and handling.

Where Standard grade makes sense

  • Short projects where each panel is used for up to about six pours.
  • Walls, columns and footings on low-rise buildings.
  • One-off or irregular formwork where panels are cut to shape and will not be reused many times anyway.
  • Tenders where panels are written off at the end of the job and replaced for the next contract.

On these jobs, a higher grade would add specification the project never uses.

Where it does not

Standard grade is not the right choice for:

  • High-rise or repetitive pours, where panels are cycled floor after floor. Look at Promax or Phenolic.
  • Steam-cured or very wet work, which needs the longer boil-test performance of Promax (48 h) or Phenolic (72 h).
  • Projects needing 8 or more uses from each panel. Premium is rated for 8–12.

If you are unsure, compare cost per pour rather than cost per sheet. Our guide to film faced plywood grades sets the four grades side by side.

Handling to reach the upper end of the reuse range

The 4–8 reuse range depends on how panels are treated on site. To reach the upper end:

  • apply release agent evenly before each pour,
  • clean panels soon after striking, without metal scrapers,
  • seal every cut edge and drilled hole before first use,
  • lift panels rather than dropping or dragging them,
  • store panels flat, off the ground and covered between pours.

Panels leave the factory with edges sealed in water-resistant paint, so only site cuts need attention. How Many Times Can Film Faced Plywood Be Reused? covers the same factors across all four grades.

FAQ

How many times can Standard film faced plywood be reused?

The Greenwood data sheet gives 4–8 reuses for Standard as a reference value. Where a panel lands in that range depends on release agent, cleaning soon after striking, careful handling, sealed cut edges and dry, flat storage between pours. Rough handling can bring it below the range.

Is Standard grade suitable for slabs?

It can be used for slab formwork on short projects where each panel sees only a few pours. For repeated slab cycles on multi-story buildings, Premium at 8–12 reuses or Promax at 15–20 is the better fit, because the panel set has to survive the whole floor-by-floor programme.

What glue does Standard grade use?

Standard uses MUF glue with 12% melamine, the lowest melamine content in the Greenwood range. It passes an 8–12 hour boiling test. Higher grades raise the melamine content to 15–18% and 25%, or switch to phenolic glue, and their boil-test hours rise accordingly.

Can I order Standard grade with my own label?

Yes. Custom labels are available on request, alongside standard packing on a pallet base or wooden blocks with PE wrap and steel strapping. Send your label artwork and marking requirements with the order so they can be confirmed in writing before production starts.

Request the Standard grade data sheet

Tell us your thickness, sheet size and expected number of pours. Our team will send the Standard grade data sheet, or recommend a higher grade if your project needs it.

Request Standard data sheet →

✉ qc@fomexgroup.vn

☎ +84 877 034 666 (WhatsApp)

FOMEX Global Standard Form film faced plywood →

Greenwood film faced plywood is a product line of FOMEX Global, part of FOMEX Group.